Skip to content

Softwood · North America

Atlantic white-cedar: hardness, strength and shrinkage

Atlantic white-cedar has a Janka hardness of 350 lbf, stiffness of 0.93 million psi and bending strength of 6,800 psi (USDA Wood Handbook). It weighs about 22.4 lb per cubic foot at 12% moisture and shrinks 5.4% across the growth rings from green to dry.

Janka hardness
350 lbf
162nd of 168
Stiffness (E)
0.93 million psi
179th of 184
Bending strength
6,800 psi
180th of 184
Crushing strength
4,700 psi
Specific gravity
0.32
176th of 183
Weight at 12%
22.4 lb/ft³
1.86 lb per board foot
Shrinkage, green to dry
5.4% across rings
2.9% along them

Check a shelf in atlantic white-cedarHow much does it move?Compare all 184 woods

How it compares

At 350 lbf, atlantic white-cedar is a soft wood: 26% as hard as white oak (1,360 lbf), and 162nd of 168 for hardness among the woods that were Janka tested. Under about 700 lbf a floor or tabletop dents from a dropped fork; above 1,200 it takes everyday knocks.

Its stiffness of 0.93 million psi is 179th of 184, and white oak's is 1.78. Stiffness, not strength, decides how far a shelf or rail bends under a load; strength decides when it breaks. Its bending strength is 6,800 psi, 45% of white oak's.

Will a shelf of it sag?

A 3/4-inch shelf, 11 1/4 inches deep (a 1×12), carrying 20 pounds per foot, stays under the 1/600 "looks bent" limit after several years for spans up to about 25" in atlantic white-cedar. Longer than that and it will visibly bow; thicker stock, a front edge strip or a middle support fixes it. Estimated Worked out from the Handbook's stiffness with the creep allowance used in the shelf sag calculator; it is a woodworker's rule of thumb, not a structural check.

Enter your own span, depth and load.

How much it moves

Across the growth rings (plainsawn faces) it shrinks 5.4% from green to oven dry; along them (quartersawn faces) 2.9%; in volume 8.8%. Between a dry winter room (30% humidity, about 6.2% moisture) and a humid summer one (60%, about 11.0%) a 12-inch plainsawn board changes width by about 0.11 inch, and a quartersawn one by about 0.06 inch. Try your own width and humidity.

Weight

At 12% moisture it weighs about 22.4 pounds per cubic foot, or 1.86 pounds per board foot. A 1×6 board 8 feet long (4 board feet) comes to roughly 7.5 pounds. Green lumber weighs more, because the water has not dried out.