Douglas-fir (interior west): hardness, strength and shrinkage

Douglas-fir (interior west) has a Janka hardness of 660 lbf, stiffness of 1.83 million psi and bending strength of 12,600 psi (USDA Wood Handbook). It weighs about 35.0 lb per cubic foot at 12% moisture and shrinks 7.5% across the growth rings from green to dry.

Janka hardness
660 lbf
113th of 168
Stiffness (E)
1.83 million psi
62nd of 184
Bending strength
12,600 psi
97th of 184
Crushing strength
7,430 psi
Specific gravity
0.5
103rd of 183
Weight at 12%
35.0 lb/ft³
2.91 lb per board foot
Shrinkage, green to dry
7.5% across rings
4.8% along them

Check a shelf in douglas-fir (interior west)How much does it move?Compare all 184 woods

How it compares

At 660 lbf, douglas-fir (interior west) is a soft wood: 49% as hard as white oak (1,360 lbf), and 113th of 168 for hardness among the woods that were Janka tested. Under about 700 lbf a floor or tabletop dents from a dropped fork; above 1,200 it takes everyday knocks.

Its stiffness of 1.83 million psi is 62nd of 184, and white oak's is 1.78. Stiffness, not strength, decides how far a shelf or rail bends under a load; strength decides when it breaks. Its bending strength is 12,600 psi, 83% of white oak's.

Will a shelf of it sag?

A 3/4-inch shelf, 11 1/4 inches deep (a 1×12), carrying 20 pounds per foot, stays under the 1/600 "looks bent" limit after several years for spans up to about 31" in douglas-fir (interior west). Longer than that and it will visibly bow; thicker stock, a front edge strip or a middle support fixes it. Estimated Worked out from the Handbook's stiffness with the creep allowance used in the shelf sag calculator; it is a woodworker's rule of thumb, not a structural check.

Enter your own span, depth and load.

How much it moves

Across the growth rings (plainsawn faces) it shrinks 7.5% from green to oven dry; along them (quartersawn faces) 4.8%; in volume 11.8%. Between a dry winter room (30% humidity, about 6.2% moisture) and a humid summer one (60%, about 11.0%) a 12-inch plainsawn board changes width by about 0.15 inch, and a quartersawn one by about 0.10 inch. Try your own width and humidity.

Weight

At 12% moisture it weighs about 35.0 pounds per cubic foot, or 2.91 pounds per board foot. A 1×6 board 8 feet long (4 board feet) comes to roughly 11.7 pounds. Green lumber weighs more, because the water has not dried out.