Skip to content

Hardwood · Americas

Manbarklak: hardness, strength and shrinkage

Manbarklak has a Janka hardness of 3,480 lbf, stiffness of 3.14 million psi and bending strength of 26,500 psi (USDA Wood Handbook). It weighs about 60.8 lb per cubic foot at 12% moisture and shrinks 10.3% across the growth rings from green to dry.

Janka hardness
3,480 lbf
3rd of 168
Stiffness (E)
3.14 million psi
7th of 184
Bending strength
26,500 psi
5th of 184
Crushing strength
11,210 psi
Specific gravity
0.87
7th of 183
Weight at 12%
60.8 lb/ft³
5.07 lb per board foot
Shrinkage, green to dry
10.3% across rings
5.8% along them

Check a shelf in manbarklakHow much does it move?Compare all 184 woods

How it compares

At 3,480 lbf, manbarklak is a very hard wood: 256% as hard as white oak (1,360 lbf), and 3rd of 168 for hardness among the woods that were Janka tested. Under about 700 lbf a floor or tabletop dents from a dropped fork; above 1,200 it takes everyday knocks.

Its stiffness of 3.14 million psi is 7th of 184, and white oak's is 1.78. Stiffness, not strength, decides how far a shelf or rail bends under a load; strength decides when it breaks. Its bending strength is 26,500 psi, 174% of white oak's.

Will a shelf of it sag?

A 3/4-inch shelf, 11 1/4 inches deep (a 1×12), carrying 20 pounds per foot, stays under the 1/600 "looks bent" limit after several years for spans up to about 37" in manbarklak. Longer than that and it will visibly bow; thicker stock, a front edge strip or a middle support fixes it. Estimated Worked out from the Handbook's stiffness with the creep allowance used in the shelf sag calculator; it is a woodworker's rule of thumb, not a structural check.

Enter your own span, depth and load.

How much it moves

Across the growth rings (plainsawn faces) it shrinks 10.3% from green to oven dry; along them (quartersawn faces) 5.8%; in volume 15.9%. Between a dry winter room (30% humidity, about 6.2% moisture) and a humid summer one (60%, about 11.0%) a 12-inch plainsawn board changes width by about 0.22 inch, and a quartersawn one by about 0.12 inch. Try your own width and humidity.

Weight

At 12% moisture it weighs about 60.8 pounds per cubic foot, or 5.07 pounds per board foot. A 1×6 board 8 feet long (4 board feet) comes to roughly 20.3 pounds. Green lumber weighs more, because the water has not dried out.

Similar woods

All 184 woods

Report a problem with this page