Skip to content

Hardwood · North America

Swamp white oak: hardness, strength and shrinkage

Swamp white oak has a Janka hardness of 1,620 lbf, stiffness of 2.05 million psi and bending strength of 17,700 psi (USDA Wood Handbook). It weighs about 50.3 lb per cubic foot at 12% moisture.

Janka hardness
1,620 lbf
37th of 168
Stiffness (E)
2.05 million psi
41st of 184
Bending strength
17,700 psi
36th of 184
Crushing strength
8,600 psi
Specific gravity
0.72
22nd of 183
Weight at 12%
50.3 lb/ft³
4.20 lb per board foot

Check a shelf in swamp white oakCompare all 184 woods

How it compares

At 1,620 lbf, swamp white oak is a hard wood: 119% as hard as white oak (1,360 lbf), and 37th of 168 for hardness among the woods that were Janka tested. Under about 700 lbf a floor or tabletop dents from a dropped fork; above 1,200 it takes everyday knocks.

Its stiffness of 2.05 million psi is 41st of 184, and white oak's is 1.78. Stiffness, not strength, decides how far a shelf or rail bends under a load; strength decides when it breaks. Its bending strength is 17,700 psi, 116% of white oak's.

Will a shelf of it sag?

A 3/4-inch shelf, 11 1/4 inches deep (a 1×12), carrying 20 pounds per foot, stays under the 1/600 "looks bent" limit after several years for spans up to about 32" in swamp white oak. Longer than that and it will visibly bow; thicker stock, a front edge strip or a middle support fixes it. Estimated Worked out from the Handbook's stiffness with the creep allowance used in the shelf sag calculator; it is a woodworker's rule of thumb, not a structural check.

Enter your own span, depth and load.

Weight

At 12% moisture it weighs about 50.3 pounds per cubic foot, or 4.20 pounds per board foot. A 1×6 board 8 feet long (4 board feet) comes to roughly 16.8 pounds. Green lumber weighs more, because the water has not dried out.

Similar woods

All 184 woods

Report a problem with this page