Cherrybark oak has a Janka hardness of 1,480 lbf, stiffness of 2.28 million psi and bending strength of 18,100 psi (USDA Wood Handbook). It weighs about 47.5 lb per cubic foot at 12% moisture.

Janka hardness
1,480 lbf
43rd of 168
Stiffness (E)
2.28 million psi
20th of 184
Bending strength
18,100 psi
31st of 184
Crushing strength
8,740 psi
Specific gravity
0.68
31st of 183
Weight at 12%
47.5 lb/ft³
3.96 lb per board foot

Check a shelf in cherrybark oakCompare all 184 woods

How it compares

At 1,480 lbf, cherrybark oak is a hard wood: 109% as hard as white oak (1,360 lbf), and 43rd of 168 for hardness among the woods that were Janka tested. Under about 700 lbf a floor or tabletop dents from a dropped fork; above 1,200 it takes everyday knocks.

Its stiffness of 2.28 million psi is 20th of 184, and white oak's is 1.78. Stiffness, not strength, decides how far a shelf or rail bends under a load; strength decides when it breaks. Its bending strength is 18,100 psi, 119% of white oak's.

Will a shelf of it sag?

A 3/4-inch shelf, 11 1/4 inches deep (a 1×12), carrying 20 pounds per foot, stays under the 1/600 "looks bent" limit after several years for spans up to about 34" in cherrybark oak. Longer than that and it will visibly bow; thicker stock, a front edge strip or a middle support fixes it. Estimated Worked out from the Handbook's stiffness with the creep allowance used in the shelf sag calculator; it is a woodworker's rule of thumb, not a structural check.

Enter your own span, depth and load.

Weight

At 12% moisture it weighs about 47.5 pounds per cubic foot, or 3.96 pounds per board foot. A 1×6 board 8 feet long (4 board feet) comes to roughly 15.8 pounds. Green lumber weighs more, because the water has not dried out.